Solutions / Bouquet wrapping

How to Keep Kraft Bouquet Wrap from Splitting at the Fold

Start with two matching bouquets. Keep one wrap dry and expose the other to the stem contact it will see in transit. A fold that splits during dry assembly calls for a different trial from one that fails only after wetting.

Request paper samples
Two bouquets with folded brown outer wraps and tied ribbons
Bouquet wrapping reference. Ribbon lettering was removed from the supplied photo.

Find the first point of failure

What you seeWhat to tryHow to check it
The point splits as you pull the wrap tightEase the tightest corner or shift the overlap so the pull falls on a wider area.Repeat with the same paper, sheet size and bouquet. Inspect the corner immediately after tying.
The fold survives packing but tears near damp stemsCheck whether the stem pouch leaks or condensation can reach the fold. Keep the outer wrap clear of the wet area.Repeat with the intended stem protection. Inspect the fold after the usual holding time and after lifting the bouquet.
One fold direction splits more often on dry samplesRotate the same sheet by 90 degrees for a second trial. Confirm grain direction with the supplier if the result changes.Keep the shape, overlap and tie position the same. Compare the first tear location on both wraps.

Choose the material by how the fold fails

Failure on the sampleMaterial to trialWhat to verify
The dry fold splits as the wrap is pulled tightTrial YoungSun’s high-tensile kraft. Where the fold needs more give, ask for an extensible kraft candidate.Request tensile and elongation in both machine and cross directions. Keep the fold and sheet size fixed, then compare both grain orientations and confirm the paper still folds neatly.
Drips or condensation reach the wrap from the stemsTrial film-coated or laminated kraft with the protected face towards the moisture source.Inspect the finished fold, overlap and exposed cut edges after the intended holding time. Check for moisture reaching the paper, film separation at the crease and a closure that slips.
The sheet gets damp and still has to support handlingAsk for wet-strength kraft made with a wet-strength additive in the furnish.Request wet tensile values with the test method and exposure conditions. Lift the wrapped bouquet after the expected wet contact and inspect the loaded fold. Confirm the proposed grade and availability.

Use your current wrap as the baseline. If you need an uncoated reference, YoungSun’s brown kraft paper data sheet lists 65, 70, 75, 80, 90 and 95 gsm. Try 65 and 80 gsm as a dry comparison to see how the wrap drapes and holds its shape. Ask for separate specifications for the high-tensile, extensible, coated or wet-strength grade you intend to trial.

Approve the wrap after handling

  1. Use your largest bouquet that will take the proposed sheet size. Keep stem protection, overlap and tie position consistent.
  2. Check each wrap immediately after folding and again after the expected holding period. Lift it and place it in the actual transport tray or carton.
  3. Record where any split starts, whether that area is damp, and whether the wrap still holds its shape. Keep a marked sample of the paper and fold pattern you approve.

Tell us what you’re wrapping

Send the bouquet dimensions, current paper weight if known, sheet size or roll width, expected quantity, and a picture of the split or fold. Tell us where moisture reaches the wrap, how long it stays there and whether you need a film barrier or a paper that can still be handled after wetting.

Ask for a kraft paper trial